PRE-ELEC ESD 7300 is a static dissipative thermoplastic compound based on PC/PBT. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 7300 has been developed for injection molding. The products made out of PRE-ELEC ESD 7300 are washable, reusable and recyclable. Surface resistance values of 108 ohms (EOS/ESD S11.11-1993, IEC 61340-5-1) can be achieved with optimum processing parameters. Typical applications include injection molded technical parts used in e.g. office machines, telecommunications and other electronic equipments to give a permanent ESD protection. Information provided by Premix Thermoplastics Inc. |