MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper Nickel Tin, UNS C72800, H04 Temper, Strip
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Hard

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Gas Shielded Arc Welding, Spot Weld, Seam Weld, Butt Weld, Capacity for Being Cold Worked; Good Suitability – Capacity for Being Hot Formed

Common Fabrication Processes: Coining; Cold Heading; Drawing; Extruding and Machining; Forming and Bending; Knurling; Roll Threading; Swaging; Welding

Typical uses: Bars; Extruded Shapes; Forgings; Rod; Springs; Tubes; Wire

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.324 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 21
@Thickness 1.60 mm
Tensile Strength 115 ksi
@Thickness 1.60 mm
Tensile Strength, Yield 90.0 ksi
@Thickness 1.60 mm
0.01% Offset
 110 ksi
@Thickness 1.60 mm
0.2% Offset
Elongation at Break 8.7 %
@Thickness 1.60 mm
Tensile Modulus 18500 ksi
Modulus of Rigidity 6840 ksi
Poissons Ratio 0.35Calculated
Machinability 10 %
Forgeability 30 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000159 ohm-cm10.8% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.50 µin/in-°F
@Temperature 20.0 - 100 °C
 8.60 µin/in-°F
@Temperature 20.0 - 200 °C
 9.10 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0910 BTU/lb-°F
Thermal Conductivity 31.7 BTU-in/hr-ft²-°F
Melting Point 1682 - 1980 °F
Solidus 1682 °F
Liquidus 1980 °F
Annealing Point 1470 - 1550 °F
 
Processing PropertiesOriginal ValueComments
Hot-Working Temperature 1200 - 1600 °F
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.10 %
Antimony, Sb <= 0.020 %
Bismuth, Bi <= 0.0010 %
Boron, B <= 0.0010 %
Copper, Cu 78.6 - 82.8 %As Balance
Iron, Fe <= 0.50 %
Lead, Pb <= 0.0050 %
Magnesium, Mg 0.0050 - 0.15 %
Manganese, Mn 0.050 - 0.30 %
Nickel, Ni 9.5 - 10.5 %
Niobium, Nb (Columbium, Cb) 0.10 - 0.30 %
Phosphorus, P <= 0.0050 %
Silicon, Si <= 0.050 %
Sulfur, S <= 0.0025 %
Tin, Sn 7.5 - 8.5 %
Titanium, Ti <= 0.010 %
Zinc, Zn <= 1.0 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC72800x6 / 293113

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.