MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials TPSiV® 4200-70A Silicone Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Silicone thermoplastic elastomer with good chemical resistance and excellent abrasion and scratch resistance.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.020 cm/cmISO 294-4, 2577
Melt Flow 27 g/10 min
@Load 10.0 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 14.5 MPaCross direction; ISO 527-1/-2 or ISO 37
Tensile Stress at Strain 3.90 MPa
@Strain 100 %
Cross direction; ISO 527-1/-2 or ISO 37
Elongation at Break >= 300 %Cross direction; ISO 527-1/-2 or ISO 37
Flexural Strength 2.40 MPaISO 178
Flexural Modulus 32.8 MPaISO 178
Tear Strength 48.6 kN/mnormal; ISO 34-1
Compression Set 22 %
@Temperature 23.0 °C
ISO 815
 75 %
@Temperature 70.0 °C,
Time 86400 sec
ISO 815
 
Processing PropertiesOriginal ValueComments
Melt Temperature 195 °COptimum, Injection
 185 - 205 °CRange, Extrusion
Mold Temperature 30.0 °COptimum, Injection
 20.0 - 40.0 °CInjection
Drying Temperature 70.0 °CInjection
 70.0 °CExtrusion
Dry Time 2.00 - 4.00 hourExtrusion, Dehumidified Dryer
 2.00 - 4.00 hourInjection, Dehumidified Dryer
 
Descriptive Properties
CompatibilityAcrylic Polymers
 Polycarbonate
 Styrenics
Drying RecommendedyesInjection
Max. screw tangential speed (m/s)0.4Injection
PolymerTPV

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSX4904 / 249183

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.