MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Armacell HT Armaflex® Industrial FEF Insulation
Categories: Other Engineering Material

Material Notes: Description: HT/Armaflex® Industrial is a flexible, high density and mechanically robust, closed cell thermal insulation material based on extruded elastomeric foam. The product has been specially developed to provide enhanced thermal resistance of the insulation systems with its low thermal conductivity.

Special features: This product us resistant to elevated operating temperatures. The product is suitable for use in multi-layer applications including Aram-Sound Industrial Systems.

Application: Thermal insulation/protection of pipes, vessels and ducts (incl. elbows, fittings, flanges etc.) in offshore, industrial (typically oil & gas) and process equipment facilities. HT/Armaflex® Industrial is also used as a component of Arma-Sound Industrial Systems to provide acoustic insulation on industrial pipework and vessels ensuring reduction of sound transmission.

Information provided by Armacell®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0593 - 0.0753 g/cc0.00214 - 0.00272 lb/in³tubes; ASTM D1622
 0.0705 - 0.0849 g/cc0.00255 - 0.00307 lb/in³sheets; ASTM D1622
Water Absorption <= 0.10 %<= 0.10 %ASTM C209
pH 7.0 - 9.07.0 - 9.0ISO 10523
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength >= 0.0152 MPa
@Strain 25 %
>= 2.20 psi
@Strain 25 %
ISO 6916-1
Tear Strength 0.400 kN/m2.28 pliISO 34-1
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  <= 0.0390 W/m-K
@Temperature -50.0 °C
<= 0.271 BTU-in/hr-ft²-°F
@Temperature -58.0 °F
EN ISO 13787
 <= 0.0410 W/m-K
@Temperature 0.000 °C
<= 0.285 BTU-in/hr-ft²-°F
@Temperature 32.0 °F
EN ISO 13787
 <= 0.0470 W/m-K
@Temperature 50.0 °C
<= 0.326 BTU-in/hr-ft²-°F
@Temperature 122 °F
EN ISO 13787
 <= 0.0570 W/m-K
@Temperature 100 °C
<= 0.396 BTU-in/hr-ft²-°F
@Temperature 212 °F
EN ISO 13787
 <= 0.0630 W/m-K
@Temperature 125 °C
<= 0.437 BTU-in/hr-ft²-°F
@Temperature 257 °F
EN ISO 13787
 <= 0.0710 W/m-K
@Temperature 150 °C
<= 0.493 BTU-in/hr-ft²-°F
@Temperature 302 °F
EN ISO 13787
Maximum Service Temperature, Air 150 °C302 °FEN 14706, EN 14707 and EN 14304
Minimum Service Temperature, Air -50.0 °C-58.0 °FEN 14706, EN 14707 and EN 14304
 
Processing PropertiesMetricEnglishComments
Shelf Life 36.0 Month36.0 Month
 
Descriptive Properties
Water Vapor Permeability<0.034 perm-inchtubes, EN 12086 and EN 13469
 <0.045 perm-inchsheets, EN 12086 and EN 13469

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PARMD163 / 186774

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.