MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Zotefoams Evazote® EV45CN Conductive Ethylene Vinyl Acetate Copolymer Foam
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstanding physical attributes.

Information provided by Zotefoams

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0370 - 0.0490 g/ccsheet density
 0.0450 g/ccNominal skin/skin; BS ISO 7214 1998
Cell Length 0.200 - 0.600 mm
 0.400 mmTypical Diameter
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore OO 5210 mm cell/cell thickness; ISO 868 1985
Tensile Strength 0.575 MPaISO 7214 1998
Elongation at Break 170 %
Compressive Yield Strength 0.0400 MPa
@Strain 10 %
BS ISO 7214 1998
 0.0610 MPa
@Strain 25 %
BS ISO 7214 1998
 0.0940 MPa
@Strain 40 %
BS ISO 7214 1998
 0.128 MPa
@Strain 50 %
BS ISO 7214 1998
Tear Strength 1.24 kN/mBS EN ISO 8067 1995
Compression Set 3.5 %
@Time 79200 sec,
Strain 25 %
24 hr recovery; BS ISO 7214 1998
 9.5 %
@Time 79200 sec,
Strain 25 %
0.5 hr recovery; BS ISO 7214 1998
 14.5 %
@Time 79200 sec,
Strain 50 %
24 hr recovery; BS ISO 7214 1998
 22 %
@Time 79200 sec,
Strain 50 %
0.5 hr recovery; BS ISO 7214 1998
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1000 ohm-cmASTM D991-89
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0380 W/m-Kmean temp of 10°C; ISO 8302 1991
Maximum Service Temperature, Air 70.0 °C
Minimum Service Temperature, Air -70.0 °C
Flammability Test 0.70
@Thickness 13.0 mm
Horizontal Burn Rate, mm/sec; ISO 7214 1998
 1.3
@Thickness 5.00 mm
Horizontal Burn Rate, mm/sec; ISO 7214 1998
 
Descriptive Properties
FlammabilityAutomotive: FMVSS.302 burn ratePass: 5mm and thicker

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zotefoams Evazote® EV120CN Conductive Ethylene Vinyl Acetate Copolymer Foam
Zotefoams Evazote® EV70CN Conductive Ethylene Vinyl Acetate Copolymer Foam
Wacker Vinnapas® 400 H Vinyl Acetate-Ethylene Copolymer
LyondellBasell Hostacom EKC 430N NAT Polypropylene Copolymer, 16% Talc Filled
LyondellBasell Hifax EYG 382P C12716 Polypropylene with Glass Fiber Filler

PZOTEF944 / 150700

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.