Production Method: Liquid oxygen is a by-product of nitrogen production from atmospheric air by means of low temperature rectification. Application: Liquid oxygen is used after its gasification for intensification of processes in different industries, for gas-flame treatment of metals and for other technical purposes. Information Provided by Kazanorgsintez |