MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Henkel Loctite® ECCOBOND UF 3810 Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Black liquid

Cure: Heat cure

Product Benefits:

  • One component
  • Fast cure at moderate temperatures
  • High Tg
  • Halogen free
  • Compatible with most Pb-free solders
  • Stable electrical performance in temperature humidity bias
  • Reworkable
  • Room temperature flow capability
Typical Package Application: Chip scale packages and BGA

LOCTITE ECCOBOND UF 3810 reworkable epoxy underfill is designed for CSP and BGA applications. It cures quickly at moderate temperatures to minimize stress to other components. When cured, this material provides excellent mechanical properties to protect solder joints during thermal cycling.

Information provided by Loctite®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.13 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Modulus 30.0 MPa
@Temperature 200 °C
Storage, Cured, DMA
 850 MPa
@Temperature 100 °C
Storage, Cured, DMA
 2990 MPa
@Temperature 25.0 °C
Storage, Cured, DMA
 3820 MPa
@Temperature -65.0 °C
Storage, Cured, DMA
Shear Strength 9.70 MPaLap, Glass Epoxy to Glass Epoxy; ISO 4587
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.87
@Frequency 2.00e+9 Hz
 3.44
@Frequency 1e+9 Hz
Dissipation Factor 0.0037
@Frequency 2.00e+9 Hz
 0.0071
@Frequency 1e+9 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 55.0 µm/m-°CCured, Below Tg
 171 µm/m-°CCured, Above Tg
Thermal Conductivity 0.290 W/m-KLaser Flash
Glass Transition Temp, Tg 102 °CCured, by TMA
 
Processing PropertiesOriginal ValueComments
Cure Time >= 8.00 min
@Temperature 130 °C
Working Life 72.0 hourWorklife, 25% increase in viscosity
Shelf Life 12.0 Month
@Temperature -20.0 °C
from date of manufacture
 
Descriptive Properties
Extractable Ionic Content (ppm)0.7Cured, Sodium (Na+), DI water, 1 hour @ 85 °C
 0.7Cured, Ammonium (NH4+), DI water, 1 hour @ 85 °C
 0.8Cured, Chloride (Cl-), DI water, 1 hour @ 85 °C
 5Cured, Calcium (Ca²+), DI water, 1 hour @ 85 °C
 NDCured, Potassium (K+), DI water, 1 hour @ 85 °C
 NDCured, Magnesium (Mg2+), DI water, 1 hour @ 85 °C
 NDCured, Nitrate (NO3), DI water, 1 hour @ 85 °C
 NDCured, Phosphite (PO3), DI water, 1 hour @ 85 °C
 NDCured, Sulfate (SO4 2-), DI water, 1 hour @ 85 °C
 NDCured, Bromide (Br-), DI water, 1 hour @ 85 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLOCT5089 / 255300

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.