MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos G60-110 HDPE  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Sheet/Thermoforming Grade

Material Notes: Ineos G60-110 is a high molecular weight, high density polyethylene homopolymer developed for sheet extrusion, thermoforming and large part blowmolding where the finished product demands outstanding physical performance. Its ASTM D1248 classification is Type IV, Class A, Category 5. This material meets the Food and Drug Administration requirements of 21CFR 177.1520.

Key Words: Sheet extrusion, thermoforming and large part blow molding
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.590 g/ccASTM D1895
Density 0.960 g/ccASTM D4883
High Load Melt Index 11 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 67ASTM D2240
Tensile Strength, Yield 28.3 MPa2 in/min (50 mm/min); ASTM D-638
Elongation at Break >= 700 %2 in/min (50 mm/min); ASTM D-638
Flexural Modulus 1.516 GPaTangent-Method 1; ASTM D790
Tensile Impact Strength 419 kJ/m²Type L, ASTM D1822
 
Thermal PropertiesOriginal ValueComments
CTE, linear 120 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °CASTM D648
Vicat Softening Point 134 °CASTM D1525
Brittleness Temperature <= -75.0 °CASTM D746
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
ProcessSheet Extrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos G60-25-144 HDPE
ASTM A572 Steel, grade 60
Chevron Phillips HiD® 99416 with Food Grade Antistat HDPE Blow Molding Resin
Bamberger Polymers Bapolene® 4062NA Polypropylene, Injection Grade
BP Amoco ACCPRO® 9644X Injection Grade Polypropylene

PSOLJB / 68181

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.