MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Silicon Bronze, Copper Alloy, UNS C87710, M07 Temper, As Continuous Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: As Sand Cast

Fabrication Properties: Good Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Spot Weld, Seam Weld, Butt Weld, Capacity for Being Hot Formed; Fair Suitability – Soldering, Brazing, Coated Metal Arc Welding, Capacity for Being Cold Worked

Applicable Specifications: As Continuous Cast – ASTM B505/B505M; Die Forging – ASTM B283/B283M; Ingot – ASTM B30; Rod, Bar & Shapes – Forgings ASTM B124/B124M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.301 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 14.5
@Load 3000 kg
Tensile Strength 50.8 ksiTypical
 36.3 - 65.3 ksi
Tensile Strength, Yield 14.5 - 29.0 ksi0.2% Offset
 21.8 ksi0.2% Offset, Typical
Elongation at Break 2.9 %
Machinability 70 %
Forgeability 80 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 1562 - 1742 °F
Solidus 1562 °F
Liquidus 1742 °F
 
Component Elements PropertiesOriginal ValueComments
Antimony, Sb <= 0.10 %
Copper, Cu >= 84 %
Iron, Fe <= 0.50 %
Lead, Pb <= 0.090 %
Manganese, Mn <= 0.80 %
Nickel, Ni <= 0.25 %
Phosphorus, P <= 0.15 %
Silicon, Si >= 3.0 %
Zinc, Zn 9.0 - 11 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC87710x1 / 292561

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.