Inconel Filler Metal 62 is a nickel chromium alloy designed for welding nickel base alloy 600 in up to 2" thicknesses using the gas tungsten arc, gas metal arc and submerged arc processes. Filler Metal 82 is recommended for sections exceeding 2". Information provided by Universal Wire Works for their line of welding wire and filler metal. |