A fractional melt low density polyethylene Typical Applications: - Produce bags
- Frozen foods and dry goods packaging
- Case shrink wrap, bundling
- Laminations
- General purpose clarity packaging
Features: - Excellent optics and impact strength
- High coefficient of friction
- Slip: zero
- Antiblock: 2500 ppm
Information provided by Southern Polymer |