Pyrotek B-3 is a highly versatile calcium silicate board for use in a variety of machined shapes and general purpose applications. Among its uses, Pyrotek B-3 is established as the industry standard for high efficiency furnace insulation. Our machine shops are equipped with CNC tooling equipment to produce complex components to customer specifications. Applications - Floats
- Machined spouts
- Baffle plates
- Dams
- Trough liners
- Transition plates
Advantages - Asbestos-free
- Low thermal conductivity
- Resistant to thermal shock
- Non-wetting
- Good machining characteristics
Information provided by Pyrotek. |