MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ravago Manufacturing Americas Hylex® P1010G10FR Polycarbonate, 10% Glass Fiber Reinforced  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 10% Glass Filled

Material Notes:

Information provided by Ravago

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.25 g/ccASTM D792
Water Absorption 0.14 %24 hrs; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cmASTM D955
Melt Flow 7.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 5.0 - 9.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 85ASTM D785
Tensile Strength at Break 12000 psiASTM D638
Elongation at Break 13 %ASTM D638
Flexural Strength 18000 psiASTM D790
Flexural Modulus 500000 psiASTM D790
Izod Impact, Notched 2.00 ft-lb/in73°F, 0.125 in; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.00e+16 ohm-cmASTM D257
Dielectric Strength 410 V/milin Air, 0.125 in; ASTM D149
Arc Resistance 120 secASTM D495
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 295 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 290 °FUnannealed; ASTM D648
Vicat Softening Point 310 °FASTM D1525
Flammability, UL94 V-0
@Thickness 1.14 mm
All Opaque
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 550 - 570 °F
Middle Barrel Temperature 550 - 590 °F
Front Barrel Temperature 560 - 600 °F
Nozzle Temperature 560 - 600 °F
Melt Temperature 570 - 610 °F
Mold Temperature 180 - 240 °F
Drying Temperature 250 °F
Dry Time 4 - 12 hour
Moisture Content <= 0.020 %
Injection Pressure 1200 - 1800 psi
Back Pressure 60.0 - 150 psi
Shot Size 40 - 60 %
Screw Speed 40 - 70 rpm
 
Descriptive Properties
Holding Pressure800 to 1200 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ravago Manufacturing Americas Hylex® P1010G10 HB Polycarbonate, 10% Fiberglass Reinforced
Ravago Manufacturing Americas Hylex® P1010G15 HB Polycarbonate, 15% Fiberglass Reinforced
Entec Hylex® P1010L1 HB Polycarbonate
Kotec Carbotex KG-15MRA Polycarbonate, 15% Glass Fiber Reinforced
Mitsubishi Xantar® G2F 23 R Polycarbonate-10% Glass Reinforced

PENTA036 / 36047

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.