Molding Grade PCFR, with Elevated RTI’s and (f2). All Colors but Clear. Including 50% Certified Recycled Content Materials. Polycarbonate (PC), "ReStart" furnished as pellets. May be used to produce molded or extruded articles or as a component of other industrial products.Information provided by Star Plastics. |