MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Schott LG-680 Silicate Laser Glass
Categories: Ceramic; Glass; Optical

Material Notes: LG-680 is the classic lithium-aluminum based glass with high cross section for stimulated emission, high ultraviolet transmission and high resistance to solarization.

Information provided by SCHOTT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.54 g/cc
 
Chemical PropertiesOriginal ValueComments
Acid Class, SR 1.0
Alkali Class, AR 1.0
Stain Resistance Class, FR 0.00
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 6200.1/20
Modulus of Elasticity 90.1 GPa
Poissons Ratio 0.242
Fracture Toughness 0.860 MPa-m½KIC
Shear Modulus 36.3 GPaCalculated
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.30 µm/m-°C
@Temperature 20.0 - 40.0 °C
 10.18 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.920 J/g-°C
Thermal Conductivity 1.19 W/m-K
@Temperature 25.0 °C
 1.35 W/m-K
@Temperature 90.0 °C
Transformation Temperature, Tg 468 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.57
 1.558
@Wavelength 1054 nm
 1.568
@Wavelength 633 nm
Transmission, Visible 57.51 %
 
Descriptive Properties
Climatic resistance4
Thermal Diffusivity5.09 [10-7 m2/sec]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ohara S-PHM52 Optical Glass
Ohara L-TIM28 Low Tg Optical Glass
Schott N-SF4 Glass
Schott LF5G19 597399.330, Optical Glass
Schott BG34 Conversion Filter

CSGT9937 / 183190

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.