Temper: Mill-hardened Temper, TM - SHM Fabrication Properties: Excellent Suitability – Capacity for Being Cold Worked; Good Suitability – Soldering, Brazing, Spot Weld, Capacity for Being Hot Formed; Fair Suitability – Gas Shielded Arc Welding, Coated Metal Arc Welding, Seam Weld, Butt Weld Common Fabrication Processes: Blanking; Drilling; Forming and Bending; Tapping; Turning Typical uses: Connectors; Fuse Clips; Relay Parts; Switch Parts; Fasteners; Die casting plunger tips; Resistance and Spot Welding Tips; Resistance Welding Equipment; Seam Welding Dies; Springs; Tooling for Plastic Molds; Stressed Parts Applicable Specifications: Bar – ASTM B441, ASTM B534; Forgings & Extrusions – ASTM B870; Plate – ASTM B534; Rod – ASTM B441, SAE J463, SAE J461; Seamless Tube – ASTM B937; Shapes – SAE J461, SAE J463; Sheet – ASTM B534; Strip – MILITARY MIL-C-81021, ASTM B534, SAE J461, ASTM B888/B88M, SAE J463; Tube – SAE J463, SAE J461 |