MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Jilin Xingyun Chemical XY-1 Corrosion inhibitor
Categories: Other Engineering Material

Material Notes: The product is of alkaline, a compound showing the characteristics of antisepsis and corrosion inhibition. The product finds a wide application in light oil distillate equipment for antisepsis and corrosion inhibition in atmospheric and vacuum distillation unit, hydrogenation and visbreaking facilities in the oil refinery instead of former “three injection” process. In terms of application and performance, the product is simple to dose and easy to prepare for antisepsis and corrosion inhibition, while regulating the PH value in condensate water separated from light oil is bigger than 6.0 which can make the rate of corrosion inhibition bigger than 90%. The adding of the product will not result in crystals or sediments. Therefore, there is no worry about blocking in pipelines or pollution to the environment.

Information provided by Jilin Xingyun Chemical Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density <= 1.10 g/cc
 
Component Elements PropertiesOriginal ValueComments
Nitrogen, N <= 16 %
 
Descriptive Properties
AppearanceColorless or light yellow transparency liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PJILINX055 / 317902

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.