MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NOVA Chemicals DYLITE® F271T Expandable Polystyrene Resin
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: Cup and Container Grade

Features:

  • Highly consistent bead size
  • High gloss characteristics
  • Low energy consumption
  • Fast molding cycles
  • Food contact compliant

Applications:

  • Drinking cups (hot and cold)
  • Noodle bowls
  • Take-out containers
  • Ice cream containers
  • Thin-wall cups at high density
  • Labeled and printed cups

Attributes:

  • Good thermal insulation
  • Superior temperature retention
  • Less exterior condensation
  • Strong and lightweight
  • Superior taste and odor properties

The thermal conductivity of expanded polystyrene at an average temperature of 75°F (24°C) is lowest at 3.5 pounds per cubic foot (pcf). It rises slightly at lower density until about 1.5 pcf where it increases rapidly. The rate of increase is much less at higher densities:

  • 8.0 pcf (128 g/l) - 0.269 Btu-in/(hr-ft2-°F) or 38.7 mW/(m-K)
  • 12.0 pcf (192 g/l) - 0.276 Btu-in/(hr-ft2-°F) or 39.8 mW/(m-K)

United States: DYLITE F271T complies with the U.S.A. Food and Drug Administration (FDA) Code of Federal Regulations 21 CFR 177.1640 for polystyrene and 21 CFR 178.3010 for blowing agents. Thus, DYLITE F271T may be used in the United States as an article or a component of an article intended for use in contact with food, subject to any limitations described in the regulations.

Canada: NOVA Chemicals has received a letter from the Health Products and Food Branch indicating no objection to the use in Canada of DYLITE F271T for a variety of food packaging applications.

Europe: DYLITE F271T complies with the European Union's food contact regulations including the Framework Regulation (EC) No. 1935/2004, Regulation (EC) No. 2023/2006 (GMP) and Regulation (EU) No. 10/2011, as amended, Annex I (including Table 1, Union list of authorized substances) and Annex II.

NOVA Chemicals EPS resins are biologically and chemically inert. NOVA Chemicals EPS resins are do not contain CFC's (Chlorofluorocarbons).

Information provided by NOVA Chemicals®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 38.0 - 40.0 lb/ft³
Density 0.0433 g/ccBatch Pre-Expander
 0.0481 g/ccContinuous Pre-Expander
Filler Content 5.6 %Targeted Pentane Content
 5.3 - 5.9 %Pentane Content
Particle Size 300 - 500 µm"T" Bead Size - Fine
 400 µmMean Unexpanded Bead Size
 
Thermal PropertiesOriginal ValueComments
CTE, linear 35.0 µin/in-°F
Thermal Conductivity 0.235 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 175 °F
 
Compliance PropertiesOriginal ValueComments
European Food 1935/2004 Yes
FDA YesSee notes for details.
 
Descriptive Properties
Pre-Expansion Lube Levels(%)0.09 to 0.12
Pre-Puff Age Time (Hours)2-8
Thermal Resistance (per inch)4.2(R-Value)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOVB137 / 194745

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.