MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Ineos R35C-03 PP Random Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Product Description: R35C-03 is a high flow rate, ultra-high clarity, lubricated and antistatic random copolymer designed for high-speed injection molding of medium to thin walled parts requiring excellent clarity, fast cycle times and ease of de-nesting. Finished parts produced with R35C-03 will exhibit a bluish hue, giving a look of enhanced clarity.
Availability: North America
Additive: Antistatic; Lubricant
Features: Antistatic; Fast Molding Cycle; Food Contact Acceptable; High Clarity; High Flow; Lubricated; Random Copolymer
Uses: Thin-walled Parts
Agency Rating: EC 1907/2006 (REACH); FDA 21 CFR 177.1520
RoHS Compliance: Contact Manufacture
Appearance: Clear/Transparent
Forms: Pellets
Processing Method: Injection Molding

Information provided by INEOS Olefins & Polymers USA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccASTM D792
Melt Flow 35 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 82Injection Molded; ASTM D785
Tensile Strength at Break 2410 psi2.0 in/min, Injection Molded; ASTM D638
Tensile Strength, Yield 4260 psi2.0 in/min, Injection Molded; ASTM D638
Elongation at Break >= 400 %2.0 in/min, Injection Molded; ASTM D638
Elongation at Yield 14 %2.0 in/min, Injection Molded; ASTM D638
Flexural Modulus, 1% Secant 158000 psiInjection Molded; ASTM D790A
Izod Impact, Notched 1.10 ft-lb/inInjection Molded; ASTM D256
Izod Impact, Notched (ISO) 2.74 ft-lb/in²Area, Injection Molded; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 172 °FUnannealed, Injection Molded; ASTM D648
Vicat Softening Point 264 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 7.0 %
@Thickness 1.27 mm
Injection Molded; ASTM D1003
Gloss 96 %60°, Injection Molded; ASTM D2457
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PINEOSA061 / 268297

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.