MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Trinseo PULSE™ 2100 LG PC/ABS Engineering Resin
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: PULSE™ 2100LG Engineering Resin in designed to provide top performance in tough applications, from single piece items to intricate components. Ideal for energy management solutions, it can withstand high and low temperature extremes and rapid, repeated temperature fluctuations.

Benefits:

  • Low gloss appearance
  • Low temperature ductility
  • Wide range of performance
  • Superior processability
  • Lot to lot consistency
  • Good chemical resistance
Applications:
  • Mid (floor) consoles
  • Instrument Panel components
  • Door panel trim
  • Pillars
  • Storage/load floors/glove box
Automotive Specifications:
  • 3M 11-0003-5762-1
  • CHRYSLER MS-DB-195 CPN3964
  • FORD WSS-M4D924-B1
  • GM GMW15581P-ABS+PC-T1
  • VOLKSWAGEN TL 522-31-A
  • VOLKSWAGEN TL 522-31-B

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccISO 1183/B
Water Absorption 0.15 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Linear Mold Shrinkage 0.0060 in/inISO 294-4
Linear Mold Shrinkage, Flow 0.0060 in/inASTM D955
Melt Flow 5.0 g/10 min
@Load 3.80 kg,
Temperature 260 °C
ASTM D1238
 7.8 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 53.8 MPa
@Thickness 3.20 mm
Injection Molded; ASTM D638
Tensile Strength, Yield 51.0 MPaISO 527-2
 53.1 MPa
@Thickness 3.20 mm
Injection Molded; ASTM D638
Elongation at Break 120 %ISO 527-2
 1230 %
@Thickness 3.20 mm
Injection Molded; ASTM D638
Elongation at Yield 4.5 %ISO 527-2
 5.0 %
@Thickness 3.20 mm
Injection Molded; ASTM D638
Tensile Modulus 2500 MPaISO 527-2/50
 2340 MPa
@Thickness 3.20 mm
Injection Molded; ASTM D638
Flexural Strength 78.0 MPaISO 178
 80.7 MPa
@Thickness 3.20 mm
Injection Molded; ASTM D790
Flexural Modulus 2300 MPaISO 178
 2340 MPaInjection Molded; ASTM D790
Izod Impact, Notched 530 J/m
@Temperature -29.0 °C
Injection Molded; ASTM D256
 640 J/m
@Temperature 23.0 °C
Injection Molded; ASTM D256
Izod Impact, Notched (ISO) 24.0 kJ/m²-40; ISO 180
 32.0 kJ/m²-30; ISO 180
 52.0 kJ/m²23; ISO 180
Dart Drop, Total Energy 56.5 J
@Temperature 23.0 °C
Peak, 6.6 m/sec; ASTM D3763
 62.1 J
@Temperature -29.0 °C
Peak, 6.6 m/sec; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 74.0 µm/m-°C
@Temperature -40.0 - 82.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 128 °CUnannealed; ISO 75-2/B
 129 °C
@Thickness 3.20 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 106 °CUnannealed; ISO 75-2/A
 107 °C
@Thickness 3.20 mm
Unannealed; ASTM D648
Vicat Softening Point 128 °CISO 306/B50
 142 °CISO 306/A120
 143 °CRate A (50°C/h), Loading 2 (50 N); ASTM D1525
 
Optical PropertiesOriginal ValueComments
Gloss 25 %Gardner, 60°, Smooth; ASTM D542

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo MAGNUM™ 3325 MT Acrylonitrile Butadiene Styrene (ABS) Resin
Trinseo PULSE™ 2000 EZ PC/ABS Engineering Resin
Celanese SO.F.TER Reblend® 6520OP Unreinforced PC/ABS alloy
Celanese Zytel® FR7026V0F NC010 PA66-FR(30)
Lotte Advanced Materials Starex® MP-0160R Metal Plating Grade ABS

PDWST084 / 142293

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.