MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials VTR 8505 Peroxide Cured Fluoroelastomer (FKM) Formulation  (discontinued **)
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: VTR-8505 is a 64% fluorine, peroxide-cured, low-temperature Viton® fluoroelastomer similar to VTR-8500 but with a significantly lower gum polymer viscosity of ~25 (ML at 121°C). VTR-8505 utilizes Advanced Polymer Architecture technology which includes a new peroxide cure site along with an optimized molecular weight distribution designed to deliver a polymer which:
  • Is ideal for blending with VTR-8500 to reach intermediate viscosity ranges
  • Cures exceptionally fast to a high state of cure
  • Shows improved mold release/mold fouling properties compared to Viton® GLT and GLT-305
  • Shows improved mold flow and less shear sensitivity than 65 Mooney VTR-8500
  • Shows excellent physical properties with high elongation, both original and aged
  • Shows similar heat, fluids, and low temperature resistance compared to Viton® GLT and GLT-305
  • Shows improved water resistance/volume swell in water compared to Viton® GLT and GLT-305
  • Shows excellent compression set resistance with either low or no postcure

Information provided by manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 20
@Temperature 121 °C
ML-10 (gum)-Akron data
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 68Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Tensile Strength, Ultimate 16.2 MPaCured 7 min at 177°C and Post Cured 2 hr at 232°C
Tensile Strength, Yield 0.000700 GPa10% Modulus, Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Elongation at Break 254 %Cured 7 min at 177°C and Post Cured 2 hr at 232°C
100% Modulus 0.00370 GPa
@Strain 100 %
Cured 7 min at 177°C and Post Cured 2 hr at 232°C
Compression Set 20 %
@Temperature 200 °C
Method B, O-rings 70 hr at 200°C (Post Cured 2 hr at 232°C)
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -32.8 °CDSC, modulated
 
Component Elements PropertiesOriginal ValueComments
Fluorine, F 64 %
 
Descriptive Properties
Formulation as Tested100Viton® 8505
 3Zinc Oxide
 3Diak™ 7
 3Varox® DBPH-50
 30N990 Carbon Black

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials GLT305 Peroxide Cured Fluoroelastomer (FKM) Formulation
DuPont Mobility and Materials Kalrez® 4079 FFKM Perfluoroelastomer
DuPont Mobility and Materials Kalrez® 6375 FFKM Perfluoroelastomer
Garlock Viton® 501 Fluoroelastomer Sheet Rubber
Seals Eastern Perflas® 9295 Perfluorinated Rubber

PDVDA46 / 34015

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.