Melinex® 456 is an excellent handling, high clarity polyester film with both sides pretreated for slip. The two smooth surfaces allow easy top coating. Approvals: UL 94 VTM-2 - for 200 - 700 gauge (0.05 - 0.17mm) and Library of Congress Specification - This film meets the Library of Congress Specification Number 500-500-5/31/95 for use in archival storage. Information provided by DuPont. |