DAI-EL® G-7300EBP is a bisphenol curable, gum copolymer. It has excellent mold flow compared with copolymers of similar Mooney viscosity, which makes it well suited for compression, transfer or injection molding. DAI-EL® G-7300EBP may be used in compliance with 21 CFR 177.2600, Rubber articles intended for repeated use. Finished articles are required to comply with the end tests specified in 21 CFR 177.2600 (e) or (f), as applicable. Typical Applications: Shaft seals, gaskets, molded tubing Rheological Properties MDR 2000: Temperature: 177°C Frequency: 100 cpm Strain: 0.5° Test time: 6 min Rheological Properties ODR: Temperature: 177°C Frequency: 100 cpm Strain: 3 ° Test time: 12 min Information provided by Daikin. |