MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Phillips 66 Polytac® EP NLGI Grade 2
Categories: Fluid; Lubricant; Urea Gellant

Material Notes: Polytac EP is a high-performance, multipurpose, extreme pressure polyurea grease specially developed to provide long service life in automotive and industrial applications. It provides significant performance advantages over conventional soap-thickened greases in high-temperature, long-life and sealed-for-life applications. Polytac EP is manufactured with high-quality base oils and a non-soap, polyurea thickener. It is compounded with a non-sulfur-phosphorus EP additive that provides extra protection against wear under heavy loading for longer bearing life, without being corrosive to yellow metals. It has excellent thermal stability at high temperatures plus high shear stability for long service life. It also has excellent low-temperature pumpability, is highly resistant to water washout, and protects against rust and corrosion. Polytac EP is NLGI GC-LB certified for use as a multipurpose automotive wheel bearing and chassis lubricant.

Applications:

  • Automotive wheel bearings, chassis parts, constant-velocity (CV) joints and underhood applications, such as alternators, air conditioner compressor clutch bearings, water pumps and idler pulleys
  • Sealed-for-life bearings
  • High-speed antifriction bearings
  • Agitator bearings in washing machines
  • Equipment in steel mills and chemical plants exposed to chemical contaminants
  • Industrial applications where a high-temperature, long-life, extreme-pressure grease is required
Features/Benefits:
  • Excellent high-temperature performance
  • Excellent shear stability
  • Excellent wear protection
  • High load-carrying capacity
  • Protects against rust and corrosion
  • Excellent resistance to water washout
  • Excellent low-temperature pumpability
  • NLGI GC-LB certified

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.50 lb/gal
Viscosity Measurement 70Index
Saybolt Viscosity at 100°F 683 SUS
Saybolt Viscosity at 210°F 66 SUS
Kinematic Viscosity at 40°C (104°F) 129 cSt
Kinematic Viscosity at 100°C (212°F) 11.6 cSt
Oxidative Stability 100 hour
@Pressure 0.0345 MPa
Pressure Drop; ASTM D942
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Weld Load 400 kgASTM D2596
Four Ball Wear 0.500 mmScar Diameter; ASTM D2266
Penetration 265 - 295
Timken Test 60.0 lbOK Load; ASTM D2509
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 163 °C
Minimum Service Temperature, Air -34.0 °C
Dropping Point 260 °C
 
Descriptive Properties
ColorGreen
Copper Corrosion1aASTM D130
ThickenerPolyurea
Water Washout Resistance0.02Weight Loss @ 175°F, ASTM D1264

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5139 / 198392

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.