A neutral salt designed for heat treatment high alloy steels requiring temperatures of 1650° to 2200°F. Formulated per MIL-S-10699-B, Class 6. Information provided by Heatbath Corporation - Park Metallurgical. Heatbath/Park has been acquired by DuBois Chemicals. |