MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Versalis Greenflex® MQ 40 Ethylene Vinyl Acetate Copolymer - Injection Molding & Compounding
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate; Molded/Extruded

Material Notes: Greenflex MQ 40 is an ethylene vinyl acetate copolymer (EVA) for injection molding and compounding applications. Greenflex MQ 40 combines high fluidity and high elasticity.

Main Applications: Greenflex MQ 40 is recommended for injection molding of gaskets, ski sticks rounds, foamed and crosslinked articles.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.941 g/ccISO 1183
Vinyl Acetate Content 19 %Internal Method
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 89ISO 868/A
Hardness, Shore D 33ISO 868/A
Tensile Strength, Yield 4.00 MPaISO 527
Flexural Modulus 40.0 MPaISO 178
 
Thermal PropertiesOriginal ValueComments
Melting Point 83.0 °CInternal Method
Vicat Softening Point 56.0 °C
@Load 1.00 kg
ISO 306/A
Brittleness Temperature <= -80.0 °CASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Ateva® 1807EG Medical Grade EVA
Eurofoam Evacell EVA 50/S EVA + NR Foam
ExxonMobil Escorene® LD-760 High EVA Compounding Resin
Innospec FLEXAREN® 18000 EVA-Copolymer
LyondellBasell Alathon® M5363 High Density Polyethylene

PENG152 / 124546

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.