MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECASINT 1041 Polyimide, 30% MoS2 Filled (PI)
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Machined, MoS2 Filled

Material Notes: TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excellent wear resistance among other things. The TECASINT 2000 series offers these enhanced thermal properties along with lower moisture absorption, a higher degree of toughness, and better machining properties. TECASINT 2011 is unfilled, while TECASINT 2021 contains 15% graphite which offer improved wear resistance and a lower coefficient of friction. TECASINT 2000 series with their superior physical properties, are ideal for application in the aerospace, nuclear, automotive, electrical/electronics, and chemical processing industries.
    Main Features
  • High thermal and mechanical capacity
  • Good radiation-resistance
  • Low outgassing
  • Flame retardant according to UL94 V-0
  • Easily machined
  • Very creep resistant
  • Good slid and wear properties
  • Broad chemical compatibility
  • Good electrical insulating
  • Sensitive to hydrolysis in higher thermal range

    Applications
  • Mechanical engineering
  • Vacuum engineering
  • Aircraft and aerospace industries
  • Precision engineering
  • Cryogenics

Preferred Fields

Vacuum seal, valve seating, skid rails, chain guides, piston rings, bearings, washers

Information Provided by Ensinger, Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.67 g/cc
@Temperature 23.0 °C
DIN 53 479
Filler Content 30 %Molybdenum disulfide
Water Absorption 0.72 %
@Temperature 23.0 °C,
Time 86400 sec
EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 89
@Temperature 23.0 °C
DIN 53 505
Tensile Strength, Yield 82.0 MPa
@Temperature 23.0 °C
EN ISO 527
Elongation at Break 2.8 %
@Temperature 23.0 °C
EN ISO 527
Tensile Modulus 4340 MPa
@Temperature 23.0 °C
EN ISO 527
Flexural Strength 126 MPa
@Temperature 23.0 °C
EN ISO 178
Flexural Modulus 4330 MPa
@Temperature 23.0 °C
EN ISO 178
Flexural Strain at Yield 3.7 %EN ISO 178
Compressive Strength 204 MPa
@Temperature 23.0 °C
EN ISO 604
Charpy Impact Unnotched 2.965 J/cm²EN ISO 179
Compression Set 64 %Compression at Break; EN ISO 604
 
Thermal PropertiesOriginal ValueComments
CTE, linear 65.0 µm/m-°C
@Temperature 50.0 - 200 °C
DIN 53 752
Glass Transition Temp, Tg 330 °CDMTA
Flammability, UL94 V-0
 
Descriptive Properties
ColorBlack
DIN-AbbreviationPI M 30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ensinger TECASINT 4041 Polyimide, Glossy Black, Molybdenum Sulfide (PI)
Ensinger TECASINT 4201 SD Polyimide, Black, Carbon Fiber (PI)
Ensinger TECASINT 1021 Polyimide, 15% Graphite Filled (PI)
Ensinger TECASINT 1061 Polyimide, 15% Graphite, 10% PTFE Filled (PI)
Ensinger TECASINT 3032 Polyimide, Black, 40% Graphite (PI)

PENSIN047 / 98108

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.