MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
BNZ Materials Marinite® P High Temperature Structural Insulation
Categories: Ceramic; Oxide

Material Notes: Oven dried formulations of BNZ boards are used in a variety of heat insulating processes, fire protection and machined parts. Selection is commonly based on a balance between strength and insulating qualities. Examples include oven walls and linings, soldering insulation, fire doors, fire training burn buildings, cable trays, personnel protection, and as USCG-approved insulation for marine ships and off-shore rigs. Back-up insulation applications include ladles, torpedo cars and tundishes in the iron and steel industry, lime and cement plant rotary kilns, and aluminum die cast holding furnaces.

Information provided by BNZ Materials Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 60.0 lb/ft³
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.00960 GPa
Compressive Yield Strength 3.05 ksi
@Strain 5.0 %
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+8 ohm-cmASTM D257
Dielectric Strength 46.0 V/milASTM D495
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.160 W/m-K
@Temperature 204 °C
 0.170 W/m-K
@Temperature 316 °C
 0.170 W/m-K
@Temperature 427 °C
 0.170 W/m-K
@Temperature 538 °C
Shrinkage 0.60 %
@Temperature 649 °C,
Time 86400 sec
Length/width
 2.1 %
@Temperature 649 °C,
Time 86400 sec
Thickness
 
Component Elements PropertiesOriginal ValueComments
H2O, Water 3.0 %
 
Descriptive Properties
Screw Holding Strength227 kgat 7/8" penetration

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1141 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round
AISI 1141 Steel, as rolled
Copper, Cu; Cold Drawn
304 Stainless Steel
BNZ Materials Marinite® A Ceramic Board for Aluminum Contact

CBNZ930 / 149170

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.