MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Catalyst CT/7-LR UV LB Polyolefin based masterbatch
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Catalyst CT/7-LR UV LB is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. It is designed to minimize the blooming effect that could occur in warm areas. Developed for Polidan®, Polidiemme® and Cogegum® GFR series compounds, it is suitable for most severe long term ageing conditions. It has a low catalytic activity and it confers improved UV/VIS and aging resistance. Catalyst CT/7-LR UV LB can be used in a wide application range due to its catalytic activity and the anti-ageing effect given to the final product. It contains also a metal deactivator that allows its use also in direct contact with untinned copper.

Availability:

  • Asia Pacific
  • Europe
Features:
  • Copper Contact Stabilized
  • Halogen Free
Uses:
  • Wire & Cable Applications

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.520 g/ccApparent, test made on granules
 0.970 g/cctest made on pressed plate
 
Descriptive Properties
AppearanceNatural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOLVAY516 / 218244

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.