MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Solvay Chemicals Blue pigment
Categories: Fluid

Material Notes:

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size 25 - 30 µmViolet
 30 - 40 µmBlue
pH 5.5 - 7.5
Evaporation Loss <= 1.0 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity <= 1000 ohm-cmBlue
 <= 1000 ohm-cmViolet
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 0.00 %
@Wavelength 570 nm
Blue
 0.00 %
@Wavelength 580 nm
Blue 7:3
 0.00 %
@Wavelength 630 nm
Blue 9:1
 0.00 %
@Wavelength 530 nm
Violet
 0.00 %
@Wavelength 580 nm
Blue 8:2
 0.00 %
@Wavelength 580 nm
Blue 9:1
 3.0 %
@Wavelength 630 nm
Blue 8:2
 3.0 %
@Wavelength 630 nm
Blue 7:3
 3.0 %
@Wavelength 680 nm
Blue
 10 %
@Wavelength 690 nm
Blue 9:1
 10 %
@Wavelength 600 nm
Violet
 10 %
@Wavelength 630 nm
Violet
 20 %
@Wavelength 700 nm
Blue 8:2
 30 %
@Wavelength 380 nm
Blue 7:3
 30 %
@Wavelength 380 nm
Blue 8:2
 30 %
@Wavelength 380 nm
Blue 9:1
 30 %
@Wavelength 380 nm
Violet
 30 %
@Wavelength 380 nm
Blue
 65 %
@Wavelength 440 nm
Violet
 80 %
@Wavelength 460 nm
Blue 7:3
 83 %
@Wavelength 460 nm
Blue 8:2
 87 %
@Wavelength 460 nm
Blue 9:1
 90 %
@Wavelength 460 nm
Blue
IR Transmittance 5.0 %
@Wavelength 780 nm
Blue
 15 %
@Wavelength 780 nm
Blue 9:1
 25 %
@Wavelength 780 nm
Blue 8:2
 30 %
@Wavelength 710 nm
Blue 7:3
 32 %
@Wavelength 780 nm
Blue 7:3
 95 %
@Wavelength 730 nm
Violet
 
Descriptive Properties
Composition<100 ppmBa
 <300 ppmCa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WSOLV092 / 147741

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.