MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Ryton® R-4-270NA PPS, 40% glass fiber
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

Material Notes: 40% glass fiber, high mechanical strength

Ryton® R-4-270NA 40% glass fiber reinforced polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water.

Features: Chemical Resistant; Good Processability; High Strength

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.67 g/ccMethod A; ASTM D792
Water Absorption 0.020 %
@Time 86400 sec
ASTM D570
 0.020 %
@Time 86400 sec
ISO 62
Moisture Absorption 0.0600 %50% RH; ISO 62
Water Absorption at Saturation 0.090 %ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm
@Thickness 3.20 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
@Thickness 3.20 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 200 MPaISO 527-2
Elongation at Break 1.8 %ISO 527-2
Tensile Modulus 15300 MPaISO 527-2
Flexural Strength 290 MPaISO 178
Flexural Modulus 13500 MPaISO 178
Compressive Strength 285 MPaASTM D695
Izod Impact, Notched (ISO) 10.0 kJ/m²Notch A; ISO 180
Izod Impact, Unnotched (ISO) 50.0 kJ/m²ISO 180
Charpy Impact Unnotched 57.0 kJ/m²ISO 179
Charpy Impact, Notched 9.30 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Constant 4.0
@Frequency 1000 Hz
ASTM D150
 4.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 20.0 kV/mmASTM D149
Dissipation Factor 0.0020
@Frequency 1000 Hz
ASTM D150
 0.0020
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 125 secASTM D495
Comparative Tracking Index 100 - 174 VPLC 4; UL 746
 175 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 10.0 µm/m-°C
@Temperature 100 - 200 °C
ASTM E831
 15.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
ASTM E831
CTE, linear, Transverse to Flow 45.0 µm/m-°C
@Temperature -50.0 - 50.0 °C
ASTM E831
 85.0 µm/m-°C
@Temperature 100 - 200 °C
ASTM E831
Thermal Conductivity 0.320 W/m-KASTM C177
Melting Point 280 °CISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 265 °CUnannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 1.50 mm
 5VA
@Thickness 1.50 mm
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorNatural Color
FormsPellets
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4438 / 280238

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.