MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
INEOS Styrolution K-Resin® KR10 SBC
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Product Description: K-Resin® KR10 alone or in blends, can be extruded into sheet and thermoformed on conventional equipment at high output rates. The favorable economics of K-Resin® SBC, along with high productivity, have made possible tough clear disposable drinking cups, lids and other packaging applications. INEOS Styrolution has several grades of K-Resin® SBC tailored for your sheet extrusion needs. K-Resin® KR10 will process on most conventional equipment, allowing the molder to run a crystal clear bottle without expensive machine modifications, special molds, different screws, or dryers. K-Resin® SBC are blow molded in a broad range of sizes and shapes, from small pill bottles and medical drainage units, to very tall display bottles. They can also be injection blow molded into extremely high impact bottles with glass-like clarity.
Features: Excellent Clarity; Good Stiffness; Good Toughness; High Surface Gloss; Good Formability
Applications: Molded Boxes with Integral Hinges; Medical Devices; Overcaps; Displays; Blister Packaging; Bottles and Portion Packages

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Block Copolymer; Good Stiffness; Good Toughness; High Clarity; High Gloss

Uses: Bottles; Caps; Containers; Food Packaging; Medical Devices; Medical/Healthcare Applications; Packaging; Thermoforming Applications

Appearance: Clear/Transparent

Form: Pellets

Processing Method: Extrusion; Sheet Extrusion; Thermoforming

Information provided by INEOS Styrolution

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/ccASTM D792
Water Absorption 0.090 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 63ASTM D2240
Tensile Strength, Yield 3800 psiType I, 2.0 in/min; ASTM D638
Elongation at Break 230 %Type I, 2.0 in/min; ASTM D638
Tensile Modulus 240000 psiASTM D638
Flexural Yield Strength 5400 psiASTM D790
Flexural Modulus 260000 psiASTM D790
Dart Drop, Total Energy 29.5 ft-lbInstrumented; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 144 °FUnannealed; ASTM D648
Vicat Softening Point 185 °FRate B (120°C/h), Loading 1 (10 N); ASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze <= 0.90 %ASTM D1003
Gloss 162 %mold temperature 100°F; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSTYS760 / 311453

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.