MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polyram Polytron P60B08-S Polypropylene, 60% Long Glass Fiber
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 60% Glass Fiber Filler

Material Notes: Polytron P60B08-S (Single strand) is a chemically coupled polypropylene 60% long glass fiber with extra load of additives for dilution.

Information provided by Polyram.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccISO 1183
Linear Mold Shrinkage 0.0020 - 0.0045 cm/cmISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 95.0 MPaISO 527
Elongation at Break 2.5 %ISO 527
Tensile Modulus 6300 MPaISO 527
Flexural Strength 135 MPaISO 178
Flexural Modulus 6500 MPaISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²
@Temperature 23.0 °C
ISO 180
Charpy Impact Unnotched 50.0 kJ/m²
@Temperature -30.0 °C
ISO 179
 65.0 kJ/m²
@Temperature 23.0 °C
ISO 179
Charpy Impact, Notched 11.0 kJ/m²
@Temperature -30.0 °C
ISO 179
 13.0 kJ/m²
@Temperature 23.0 °C
ISO 179
 
Thermal PropertiesOriginal ValueComments
Melting Point 162 °C
Deflection Temperature at 1.8 MPa (264 psi) 150 °CISO 75
Flame Spread 38 mm/minFMVSS302

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polyram Polytron P60B04-S Polypropylene, 60% Long Glass Fiber
Polyram Polytron P60B04 Homopolymer Polypropylene, Chemically Coupled 60% Long Glass Fiber
Polyram Polytron P60B11 Homopolymer Polypropylene, Chemically Coupled 60% LGF
Polyram Polytron P60B01 Homopolymer Polypropylene, Chemically Coupled 60% LGF
PlastiComp Complet® LGF60 - PP Homopolymer Polypropylene, 60% Long Glass Fiber Reinforced

PPOLYR950 / 126747

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.