MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Superior Flux Superior No. 18 Brazing Powder Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes: Description: Superior No. 18 is designed for spelter and conventional brazing of brass, bronze, Copper Nickel alloys and steel. It is non-bubbling, flows quickly and smoothly, and draws the melting spelter or Silver brazing alloys through the joint interstices. Oxides and other impurities are floated to the surface, resulting in strong, non-porous joints.

Applications: Brazing of brass, bronze, copper, nickel, silver and steel. Mainly used for brazing of brass musical instruments, especially tubas and other large instruments.

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.70 g/cc
Volatiles <= 0.10 %
Particle Mesh Size 40 Mesh
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 704 - 982 °CBrazing Range
 
Processing PropertiesOriginal ValueComments
Shelf Life 2.00 Month
 
Descriptive Properties
ColorWhite
Form40 Mesh Powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Indium Corp. Indalloy® 84002 Flux #2 Specialty, Acid Based Liquid Flux
Indium Corp. 16-1081T Flux Thinner
Sandvik 25.10.4.L T1 Flux Cored Wire Electrodes
Wacker Silfoam® SP 150 Silicone Antifoam Emulsion
Johnson Matthey Nickelbraze™ HTN7 Nickel Based Brazing Filler Metal

NSFLUX005 / 185689

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.