MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NRI Syntho-plug™
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Description: Syntho-Plug™ is a polyurethane impregnated, water-activated foam plug used to temporarily repair hull damage ensuring a safe trip home or to mitigate spill containment. It is initially pliable to insert into void and quickly hardens to fill the void, reducing water intake, or output, from 280 GPM to less than 1 GPM. Works with fiberglass, steel, wood or aluminum, in fresh, brackish, or saltwater, and can be applied above or below the water line.

Typical Applications:

  • Thru hull damage
  • Spill containment
Benefits:
  • Ready to use
  • Simple application
  • Effective, time saving
  • No mixing, no mess
  • Sets rock hard in minutes

Information provided by NRI® Innovative Composite Solutions

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 71.0 °C
Minimum Service Temperature, Air 0.000 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 min
@Temperature 24.0 °C
Shelf Life 12.0 Month
 
Descriptive Properties
ColorWhiteUrethane
 YellowFoam

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow BETAMATE™ 7200 Polyurethane Prepolymer
Covestro Bayfit® SA513 Flexible Polyurethane Foam, 95 Index
Covestro Bayfit® SA512 Flexible Polyurethane Foam, 75 Index
Covestro Bayfit® High Density Polyurethane Flexible Molded Foam, High Density
ATG s.r.l. AU-EU Polyurethane Rubber

PNRI017 / 192033

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.