MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRICOMP™ Compound RFN16SXZ Polyamide 66 (Nylon 66)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: LNP LUBRICOMP RFN16SXZ compound is based on Nylon 6/6 resin containing 30% glass fiber, Molybdenum diSulfide (MoS2). Added features of this grade include: Heat Stabilized, Wear Resistant.

Features: Wear resistant,Heat Stabilized,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccASTM D792
 1.41 g/ccISO 1183
Moisture Absorption 0.150 - 0.250 %Injection Molding
 0.650 %23°C/50% RH/24 hrs; ASTM D570
 1.14 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0028 cm/cm24hrs; ISO 294
 0.0030 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.013 cm/cm24hrs; ASTM D955
 0.0134 cm/cm24hrs; ISO 294
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 160 MPaASTM D638
 162 MPaISO 527
Elongation at Break 2.8 %ASTM D638
 3.0 %ISO 527
Tensile Modulus 9900 MPa1 mm/min; ISO 527
 10680 MPa50 mm/min; ASTM D638
Flexural Strength 246 MPaASTM D790
 255 MPaISO 178
Flexural Modulus 8410 MPaASTM D790
 9800 MPaISO 178
Izod Impact Notched 80.0 JASTM D256
Izod Impact, Unnotched 865 J/mASTM D4812
Izod Impact, Notched (ISO) 8.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 57.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 9.00 Jpeak; ASTM D3763
Impact Test 2.00 JMultiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.43ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.48ASTM D3702 Modified: Manual
K (wear) Factor 159 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 30.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 31.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 63.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 63.1 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 261 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 220 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 249 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Zone 2 280 - 295 °C
Zone 3 295 - 305 °C
Melt Temperature 280 - 305 °CInjection Molding
Mold Temperature 95.0 - 110 °C
Drying Temperature 80.0 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81004 / 288951

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.