Nitrile/PVC Rubber, 75-85 °IRHD. Copolymer of acrylonitrile and butadiene, blended with PVC. ASTM & ISO designation = NBR. Applications: Excellent resistance to petroleum based oils and fuels. Improved resistance to ozone and weather compared to standard nitrile grades. |