Alloy 6130 (VM) is a premium quality low-alloy steel filler metal for use with the gas tungsten arc and gas metal arc processes. 6130 (VM) is used on critical weldments of low-alloy steels where the joint is capable of being heat treated to 180,000 psi tensile strength. Information provided by Universal Wire Works for their line of welding wire and filler metal. |