MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Chemlon® 830GHI Nylon 6/12, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Glass Fiber Filler

Material Notes: Notes: 830GHI is an impact modified, 30% glass fiber reinforced, heat Stabilized grade of PA612. It offers good mechanical strength and low moistures absorption.

Availability: Europe

Fillers/Reinforcement: Glass Fiber, 30% Filler by Weight

Additive: Heat Stabilizer; Impact Modifier

Features: Good Strength; Impact Modified; Heat Stabilized; Low Moisture Absorption

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/ccISO 1183
Moisture Absorption at Equilibrium 0.80 %50% RH; ISO 62
Linear Mold Shrinkage 0.010 - 0.012 in/in
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 19300 psiISO 527-2
Elongation at Break 4.0 %ISO 527-2
Flexural Modulus 979000 psiISO 178
Izod Impact, Notched (ISO) 7.10 ft-lb/in²ISO 180/1A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 347 °FUnannealed; ISO 72-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 464 - 536 °F
Middle Barrel Temperature 464 - 536 °F
Front Barrel Temperature 464 - 536 °F
Nozzle Temperature 464 - 536 °F
Melt Temperature 464 - 536 °F
Mold Temperature 176 - 194 °F
Drying Temperature 176 °F
Dry Time 2.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, Unreinforced
Overview of materials for Nylon 66, 40% Glass Fiber Filled
Overview of materials for Nylon 66, 30% Glass Fiber Filled
Overview of materials for Nylon 66, 20% Glass Fiber Filled
Overview of materials for Nylon 66, 10% Glass Fiber Filled

PTEKNQ0536 / 237027

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.