Optimum for Black and Darker Colors between 50 and 70 L value. Also suitable for colors above 70 L value. Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties of Geon HTX Ultra LA426 Tan 3725 Geon Performance Solutions was created from PolyOne in 2019. |