MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
SABIC ULTEM™ Resin 2100F Polyetherimide (PEI) (Asia)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact Compliant, NSF 51 listing. WRAS certification in recognized colors.

Features: High Stiffness,Hydrolytic Stability,Chemical Resistance,Low Smoke and Toxicity,Good Mechanicals in Broad Temperature Range,Low Creep Sensitivity,Low Shrinkage,Good metal adhesion,Amorphous,High Strength,General Purpose,High Heat Resistance,Good dimensional stability,Flame Retardant,Food Contact Acceptable

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.34 g/ccASTM D792
Water Absorption 0.21 %
@Time 86400 sec
ASTM D570
Moisture Absorption 0.0200 %Injection Molding
Water Absorption at Saturation 1.2 %ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0060 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 7.0 g/10 min
@Load 6.60 kg,
Temperature 337 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 114ASTM D785
Tensile Strength at Break 115 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 114 MPa5 mm/min; ASTM D638
Elongation at Break 6.0 %5 mm/min; ASTM D638
Tensile Modulus 4680 MPa5 mm/min; ASTM D638
Flexural Strength 199 MPabrk, 2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 5170 MPa2.6 mm/min, 100 mm span; ASTM D790
Izod Impact Notched 53.0 JASTM D256
 459 J
@Thickness 3.20 mm
reverse notched; ASTM D256
Izod Impact, Unnotched 480 J/mASTM D4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cmASTM D257
Dielectric Constant 3.5
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 27.6 kV/mm
@Thickness 1.60 mm
in oil; ASTM D149
Dissipation Factor 0.0014
@Frequency 1000 Hz
ASTM D150
 0.0046
@Frequency 2.45e+9 Hz
ASTM D150
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 100 - 175 VUL 746A
Hot Wire Ignition, HWI 30 - 60 sec
@Thickness >=1.50 mm
UL 746A
 60 - 120 sec
@Thickness >=3.00 mm
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
@Thickness >=3.00 mm
UL 746A
 15 - 30 arcs
@Thickness >=1.50 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 32.4 µm/m-°C
@Temperature -20.0 - 150 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 210 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 208 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 223 °CRate B/50; ASTM D1525
UL RTI, Electrical 170 °CUL 746B
UL RTI, Mechanical with Impact 170 °CUL 746B
UL RTI, Mechanical without Impact 170 °CUL 746B
Flammability, UL94 V-0
@Thickness >=0.410 mm
UL 94
 5VA
@Thickness >=1.90 mm
UL 94
Smoke Density 1.8Flaming, Ds 4 min; ASTM E662
Oxygen Index 47 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 345 - 400 °C
Zone 2 340 - 400 °C
Zone 3 345 - 400 °C
Melt Temperature 350 - 400 °CInjection Molding
Mold Temperature 135 - 165 °C
Drying Temperature 150 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
 24.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82590 / 290537

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.