MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco TC-W3 2-Cycle Oil
Categories: Fluid; Lubricant

Material Notes: Features

Chevron 2-Cycle Oil TC-W3 is a high quality two-stoke engine lubricant that delivers excellent performance in water-cooled and air-cooled applications. It is formulated to provide excellent lubrication and deposit control in a wide range of applications.

Chevron 2-Cycle Oil TC-W3 contains a special ashless detergent designed to minimize piston rings from sticking to keep the engine operating smoothly and efficiently. Chevron 2-Cylce Oil TC W3 will keep the engine clean of deposits and will also protect the pistons from scuffing and pre-ignition problems.

To enhance storage and transportation safety, Chevron 2-Cycle Oil TC-W3 contains a high flash solvent. This solvent also allows good mixing with gasoline at very low temperatures.

It is dyed teal blue for easy identification of fuel-oil mixtures in pre-mixed applications.

Applications

Chevron 2-Cycle Oil TC-W3 is recommended as a premium lubricant for use in two-stroke engines where the latest TC-W3 or earlier general purpose lubricants are recommended. There applications include outboard engines, snowmobiles, motorcycles, lawn mowers, scooters, golf carts, chain saws, and other two-stroke powered equipments.

Chevron 2-Cylce Oil TC-W3 is well suited for engines using oil injection systems with fuel/oil mixture ratios of up to 150:1.

Chevron 2-cycle Oil TC W3 has excellent low temperature mixing characteristics that make It very suitable for use in cold climate conditions.

Key Words: CPS Number: 226477; MSDS Number: 5484
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 31.4 °
Brookfield Viscosity 5500 cP
@Temperature -25.0 °C
Viscosity Measurement 119Viscosity Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 46.5 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 7.3 cStASTM D445
Ash 0.00 %Sulfated Ash wt%
 
Chemical PropertiesOriginal ValueComments
Total Base Number 3.8ASTM D2896
 
Thermal PropertiesOriginal ValueComments
Pour Point -30.0 °CASTM D97
Flash Point 95.0 °CASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCHEV037 / 74652

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.