MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo PULSE™ XT9215 PC/ABS Engineering Resin
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: PULSE™ XT9215 is a easy flow, high-heat, low density PC/ABS resin delivering optimized performance for automotive exterior component applications requiring low CLTE for a better dimensional stability.

Benefits:

  • Very low CLTE for an improved dimensional stability (smaller gaps) and a better fit and finish for optimal quality
  • High ductility and easy flow for more design freedom (larger/longer parts, optimized wall thickness) and better economics improved cycle time)
  • Significant density advantage (up to 10% compared to a PC PET) for lighter parts and optimized costs
  • Faster cycle times for a better process cost control
  • High gloss for painted applications with enhanced paint adhesion
Applications:
  • Spoilers
  • Exterior trims
  • Roof bows
  • Roof rails

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.25 g/ccISO 1183/B
Volatile Organic Compounds (VOC) Content 15 g/lVDA 277
Apparent Bulk Density 0.630 g/ccISO 60
Linear Mold Shrinkage 0.0030 - 0.0060 in/in
Melt Flow 22 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ISO 1133
Spiral Flow 44.0 cm
@Thickness 2.00 mm,
Temperature 260 °C
Injection Pressure: 1.8E+3 bar
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 58.0 MPaISO 527-2/50
Elongation at Break 20 %ISO 527-2/50
Tensile Modulus 4600 MPa1 mm/min; ISO 527-2
Charpy Impact, Notched 8.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 20.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 35.0 µm/m-°C
@Temperature -30.0 - 80.0 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 108 °CUnannealed; ISO 75-2/A
Vicat Softening Point 134 °CISO 306/B50
 
Processing PropertiesOriginal ValueComments
Melt Temperature 255 - 280 °C
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 120 °C
Dry Time 5.50 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo PULSE™ XT50 PC/ABS Engineering Resin
Trinseo PULSE™ A35-110 PC/ABS
Trinseo PULSE™ XT7215 PC/ABS Engineering Resin

PTRINS9088 / 197562

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.