MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Bio-fed AF-Eco® PB 950594 HL Black Biodegradable Carbon Black Masterbatch
Categories: Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: Application: In agriculture applications, mulch films are used to cover the soil in order to suppress weeds and to promote the crops growth. M•VERA® A5001 (B0090), certified “OK compost INDUSTRIAL” by TÜV AUSTRIA Belgium, is dedicated to mulch film applications. To optimize growth and harvest of the crops and to protect the film against UV radiation the natural tone of M•VERA® A5001 can be colored into black by a masterbatch during the converting process. In order to ensure a perfect dispersion enabling the film converter to produce thin films with a very high opacity BIO-FED has developed together with AF-COLOR a masterbatch grade that unifies all necessary properties to color mulch films according to the needs of the film converters: AF-Eco® PB 950594 HL Black.

Product Features:

  • Masterbatch based on biodegradable carrier with high loading level of carbon black pigment
  • TÜV AUSTRIA Belgium certified in accordance with EN 13432 (S467, “OK compost INDUSTRIAL”)
  • Packaging: 25 kg PE bags on palettes, alternative packaging on request

    Information provided by BIO-FED

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 110 - 130 °C
 
Descriptive Properties
Dosage (%)6
Temperature stability<220°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBFED022 / 250808

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.