MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ExxonMobil SAE 30 Mobilgard 300
Categories: Fluid; Lubricant

Material Notes: Mobilgard 300 by ExxonMobil is a premium quality, extra high performance system oil designed for crosshead diesel engines. High quality paraffinic base oils along with a balanced additive system provide excellent protection even for the severe operating conditions of the latest design, high-output crosshead marine diesel engines. This product has sufficient alkalinity to neutralise any strong acids which may find their way into the crankcase from the combustion of fuel sulphur, and it has enhanced load carrying ability in order to reduce wear in heavily loaded bearings.

Mobilgard 300 is recommended primarily for use as system oil in late model, high-output, crosshead diesel engines, especially those engines employing the system oil for piston cooling. It will prevent or reduce deposit formation in the piston cooling spaces, thus maintaining piston cooling efficiency and reducing the incidence of piston top burning and piston crown cracking. It will also prevent or reduce crankcase deposits and will provide outstanding protection for heavily loaded bearings. Its reserve alkalinity allows for the burning of high sulphur fuel. Good rust prevention and water separation characteristics make Mobilgard 300 an excellent system oil in older design crosshead diesel engines which have water-cooled pistons and where crankcase deposits can be a problem with lower-quality system oils.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.889 g/cc
@Temperature 15.0 °C
Viscosity Measurement 97Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 111 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 12 cStASTM D445
Ash 0.73 %Sulfated Ash, wt%; ASTM D874
 
Chemical PropertiesOriginal ValueComments
Total Base Number 5.0mgKOH/g; ASTM D2896
 
Thermal PropertiesOriginal ValueComments
Pour Point -12.0 °CASTM D97
Flash Point 266 °CASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WEXXON338 / 75763

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.