MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Meyors Chemical TBBS NS-80
Categories: Other Engineering Material

Material Notes: Product Code: MSHQD-077-02 GT
Chemical Name: Vulca Pellet NS-80
Trade Name: Vulca Pellet NS-80
CAS No.: 95-31-8

Typical Properties: A proprietary pre-dispersed 80% N-tert-butyl-2-benzothiazyl sulphenamide in a 20% elastomeric /processing aids binder. (Elastomeric binder can be SBR or EPDM).

Recommended Applications: Vulca Pellet NS-80 provides a considerably long scorch time, great processing safety and a fast full cure. It can be used as a sole accelerator for the low sulfur vulcanization or in combination with dithiocarbamate or thiuram accelerators. The vulcanizates obtained have good ageing resistance and good moduli. The curing rate of mixes containing NS-80 in combination with thiuram and Dithiocarbamate is noticeably reduced.

Information provided by Meyors Chemical INC Limited

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/cc
Mooney Viscosity <= 30
@Temperature 100 °C
ML 1+4
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 104 °CInitial
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 1.0 %
 
Descriptive Properties
AppearanceBeige granule
Assay content>80%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMEYORS012 / 316594

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.