MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Formosa Plastics Formolene® HP6000 Pipe HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: High Density Polyethylene Homopolymer for Pipe Extrusion

Formolene® HP6000 is a high quality product for homopolymer pipe extrusion applications. It has excellent stiffness and good stiffness properties.

Applications: Corrugated Pipe, Drain Tile and Composite Lumber

Information provided by Formosa Plastics Corporation, USA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.964 g/ccASTM D1505
Environmental Stress Crack Resistance 10 hourCondition B, F50; ASTM D1693
ESCR 100% Igepal® 15 - 20 hourCondition A, F50; ASTM D1693
Melt Flow 0.65 g/10 min
@Load 2.16 kg,
Temperature 190 °C
Condition E; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4400 psi2" (50mm) per min, Type IV; ASTM D638
Elongation at Break >= 300 %2" (50mm) per min, Type IV; ASTM D638
Flexural Modulus 240000 psiASTM D790
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -118 °CASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Lupolen 5461B Q471 B High Density Polyethylene (HDPE), Pipe Grade
JPJ Technologies HDPE Pipe Grade
Ipiranga Petrochem GM 7040 G HDPE
Ineos K44-15-186 Polyethylene Copolymer
LyondellBasell Alathon L 4930TC High Denisty Polyethylene

PFPCPQ060 / 150292

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.