MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Evonik TEGO® Antifoam KE 6000 Emulsion
Categories: Other Engineering Material

Material Notes: Product description: TEGO® Antifoam KE 600 is an APEO-free organic antifoam emulsion based on polyethers, containing small amounts of organomodified siloxanes for enhancing the efficiency; dilutions show excellent stability.

Application: TEGO® Antifoam KE 600 destroys foam or pre-vents foam formation reliably in aqueous media and may therefore be used in a variety of industrial applications:

  • in emulsion, suspension and micro suspension polymerization of PVC throughout all process steps, especially for S-PVC production*li> in the production of paper and paperboard
  • in process and waste water applications
  • in a multitude of other industrial applications especially if high pH stability is requested
  • Special information on this application is available on request.
Properties / Benefits: TEGO® Antifoam KE 600 outperforms conventional organic antifoams in many respects, in particular regarding dispersibility and dilution stability. Furthermore undesirable effects associated with other organic or silicone antifoams (e. g. fogging of PVC, surface defects of coated and uncoated paper) can be very much reduced or even eliminated.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/cc
pH 7.0 - 9.0
Viscosity 200 cPdynamic
 
Descriptive Properties
Appearancewhite emulsion
Content60%Active content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik BREAK-THRU® AF 9908 Surfactants
Evonik SIPERNAT® 383 DS Silica Powder
Evonik SIPERNAT® D 10 Ceramic Powder
Evonik SIPERNAT® 50 Silica Powder
Evonik SIPERNAT® 35 Silica Powder

PEVONIL554 / 196758

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.