MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nickel Tin Bronze, UNS C94700, Copper Casting Alloy, M01 Temper, As Sand Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: As Sand Cast

Casting Characteristics: Medium – Casting Yield, Effect of Section Size, Fluidity, Gassing, Shrinkage in Solidification; Low - Drossing

Fabrication Properties: Excellent Suitability – Soldering, Brazing; Good Suitability – Gas Shielded Arc Welding, Coated Metal Arc Welding; Fair Suitability – Oxyacetylene Welding

Typical uses: Circuit Breaker Parts; Bearings; Feeding Mechanisms; Gears; Nozzles; Piston Cylinders; Shift Forks; Valve Components; Wear Guides

Applicable Specifications: As Continuous Cast – Castings SAE J462, Castings SAE J461, Castings ASTM B505/B505M; As Sand Cast – Castings ASTM B763/B763M, Castings SAE J462, Castings SAE J461, Castings ASTM B584; Ingot - ASTM B30

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.320 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 85
@Load 500 kg
Tensile Strength >= 45.0 ksifor Standard
 50.0 ksiTypical
Tensile Strength, Yield >= 20.0 ksifor Standard, 0.5% Ext
 23.0 ksi0.5% Ext
Elongation at Break >= 25 %for Standard
 35 %Typical
Tensile Modulus 15000 ksi
Fatigue Strength 14000 psi
@# of Cycles 1.00e+8
Machinability 20 %
Shear Strength 38.0 ksi
Izod Impact 85.0 ft-lb
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000143 ohm-cm12% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.9 µin/in-°F
@Temperature 20.0 - 200 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 31.2 BTU-in/hr-ft²-°F
Melting Point 1660 - 1880 °F
Solidus 1660 °F
Liquidus 1880 °F
Shrinkage 1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesOriginal ValueComments
Processing Temperature 500 °FStress Relief
Solution Temperature 1425 - 1475 °F
@Time 120 sec
Water
Precipitation Temperature 580 °FAir
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.0050 %
Antimony, Sb <= 0.15 %
Copper, Cu 85 - 90 %
Iron, Fe <= 0.25 %
Lead, Pb <= 0.090 %
Manganese, Mn <= 0.20 %
Nickel, Ni 4.5 - 6.0 %
Phosphorus, P <= 0.050 %
Silicon, Si <= 0.0050 %
Sulfur, S <= 0.050 %
Tin, Sn 4.5 - 6.0 %
Zinc, Zn 1.0 - 2.5 %
 
Descriptive Properties
Proportional Limit14 ksi

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC94700x3 / 293237

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.