Characteristics: High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications: Railway signaling equipment parts Kitchen equipment ( e.g. mixers, dishwashers ) parts Components which ought to have good electric insulation in spite of exposure to humid atmosphere, etc.Information provided by Amity Thermosets Limited |